Valley Adhesives EM-420 High Temperature Application Glue Stick

Category Polymer , Adhesive , Thermoset
Manufacturer Valley Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Valley Adhesives EM-420 High Temperature Application Glue Stick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Valley Adhesives EM-420 High Temperature Application Glue StickBonds many plastics, polyolefins and light weight materials.
Physical Properties Metric English Comments
Viscosity 7575 cP
7575 cP
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
Tensile Strength, Ultimate 2.74 MPa
397 psi
Elongation at Break 268 %
268 %
Shear Strength 3.30 MPa
479 psi
Peel Strength 5.59 kN/m
31.9 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Heat Resistance Value at 2 psi.
Softening Point 202 °C
396 °F
Processing Properties Metric English Comments
Cure Time 0.117 min
0.00194 hour
Hot tack
Pot Life 0.58 min
0.58 min
Open Time
Descriptive Properties Value Comments
Color Opaque