Vicone High Performance Rubber VicoSeal™ 003R-BK High Performance EPDM Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Vicone High Performance Rubber
Trade Name VicoSeal™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vicone High Performance Rubber VicoSeal™ 003R-BK High Performance EPDM Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two Material Product:Material 1: VicoSeal™ 003R-30 DUROMaterial 2: 11 ga CRS yellow anodized natural rubber vulcanized to yellow anodized steel (RoHS Approved)Information provided by Vicone
Physical Properties Metric English Comments
Density 1.0733 g/cc
0.038775 lb/in³
ASTM D3165
Mechanical Properties Metric English Comments
Hardness, Shore D 20
20
ASTM D2240
21

@Treatment Temp. 70.0 °C,
Time 252000 sec
21

@Treatment Temp. 158 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Tensile Strength, Yield 7.60 MPa
1100 psi
ASTM D412
4.90 MPa

@Treatment Temp. 70.0 °C,
Time 252000 sec
711 psi

@Treatment Temp. 158 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Elongation at Break 705.6 %
705.6 %
ASTM D412
632.92 %

@Treatment Temp. 70.0 °C,
Time 252000 sec
632.92 %

@Treatment Temp. 158 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Compressive Modulus 0.000220 GPa

@Strain 5.00 %
0.0319 ksi

@Strain 5.00 %
0.000340 GPa

@Strain 10.0 %
0.0493 ksi

@Strain 10.0 %
0.000550 GPa

@Strain 20.0 %
0.0798 ksi

@Strain 20.0 %
0.000740 GPa

@Strain 25.0 %
0.107 ksi

@Strain 25.0 %
Compression Set 6.18 %

@Temperature 70.0 °C,
Time 79200 sec
6.18 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395
Descriptive Properties Value Comments
Color Black