Vicone High Performance Rubber VicoSil™ 909E-BK High Performance Silicone Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Vicone High Performance Rubber
Trade Name VicoSil™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vicone High Performance Rubber VicoSil™ 909E-BK High Performance Silicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Vicone
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D3165
Mechanical Properties Metric English Comments
Hardness, Shore D 89
89
ASTM D2240
95.23

@Treatment Temp. 125 °C,
Time 252000 sec
95.23

@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Tensile Strength, Yield 9.20 MPa
1330 psi
ASTM D412
7.3968 MPa

@Treatment Temp. 125 °C,
Time 252000 sec
1072.8 psi

@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Elongation at Break 194.8 %
194.8 %
ASTM D412
78.894 %

@Treatment Temp. 125 °C,
Time 252000 sec
78.894 %

@Treatment Temp. 257 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Compressive Modulus 0.00135 GPa

@Strain 5.00 %
0.196 ksi

@Strain 5.00 %
0.00236 GPa

@Strain 10.0 %
0.342 ksi

@Strain 10.0 %
0.00516 GPa

@Strain 20.0 %
0.748 ksi

@Strain 20.0 %
0.00589 GPa

@Strain 25.0 %
0.854 ksi

@Strain 25.0 %
Compression Set 6.6 %

@Temperature 100 °C,
Time 252000 sec
6.6 %

@Temperature 212 °F,
Time 70.0 hour
ASTM D395
Descriptive Properties Value Comments
Color Black