Wellman Wellamid® GF43-66/6 XE-NBK1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66/6

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 40% Glass Fiber Reinforced
Manufacturer Wellman Engineering Resins
Trade Name Wellamid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wellman Wellamid® GF43-66/6 XE-NBK1 43% Glass Fiber Reinforced, Engineering Grade Nylon 66/6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Glass Fiber Reinforced, Engineering Grade Nylon 66/6Information provided by Wellman.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO 1183-87
Filler Content 43 %
43 %
Linear Mold Shrinkage, Flow 0.0010 - 0.0050 cm/cm
0.0010 - 0.0050 in/in
ISO DIS 294-4
Linear Mold Shrinkage, Transverse 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
ISO DIS 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 175 MPa
25400 psi
ISO 527-93
Elongation at Break 2.5 %
2.5 %
ISO 527-93
Flexural Strength 260 MPa
37700 psi
ISO 178-93
Flexural Modulus 11.8 GPa
1710 ksi
ISO 178-93
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
ISO 180-93
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
ISO 75-93