Wessex Emisshield™ ST Series Nanoparticle Ceramic Coating

Category Ceramic , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Wessex Inc.
Trade Name Emisshield™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wessex Emisshield™ ST Series Nanoparticle Ceramic Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ceramic/refractory substrate application for ceramic/refractory industry. Emisshield™ nanoparticle ceramic coatings are true grey bodies.Information provided by Wessex Inc.
Optical Properties Metric English Comments
Emissivity (0-1) 0.93 - 0.96

@Temperature 1.67 - 1930 °C
0.93 - 0.96

@Temperature 35.0 - 3500 °F
1 μm to 1000 μm