Westlake 1185 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Westlake Chemical Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake 1185 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Westlake PVC 1185 resin is a low molecular weight resin with excellent clarity designed for applications such as blow molding or where high plasticizer uptake is required.Information provided by Westlake Chemical Corporation
Physical Properties Metric English Comments
Bulk Density 0.530 g/cc
0.0191 lb/in³
ASTM D1895
Particle Mesh Size 40 Mesh
40 Mesh
99.9% min; ASTM D1921
200 Mesh
200 Mesh
4.0% max; ASTM D1921
Viscosity Measurement 0.68
0.68
Inherent; ASTM D5225
1.85
1.85
Relative
Collected Volatile Condensable Material <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
K-Value 56