Zeon Chemicals HyTemp® 4053EP AR Polyacrylate Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name HyTemp®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals HyTemp® 4053EP AR Polyacrylate Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HyTemp 4053EP contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent low temperature, oil, heat and compression set resistance.Excellent balance of low-temperature properties and oil resistance.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Mooney Viscosity 23 - 31

@Temperature 100 °C
23 - 31

@Temperature 212 °F
(1+4); Zeon Test #404
Ash <= 0.50 %
<= 0.50 %
Zeon Test #873
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -42.0 °C
-43.6 °F
Gehman T100
Glass Transition Temp, Tg -40.6 - -33.7 °C
-41.1 - -28.7 °F
Descriptive Properties Value Comments
% Volume Swell 24
Curesite Dual
Gel-Mek (%), max 20
Heat Loss (%) Max 0.7