Zeon Chemicals Hydrin® T3102 Polyepichlorohydrin Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Hydrin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Hydrin® T3102 Polyepichlorohydrin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hydrin T3102 is an ethylene oxide/epichlorohydrin/allyl glycidyl ether terpolymer with high oil fuel and solvent resistance. Compounds using Hydrin T3102 typically exhibit excellent low and high temperature properties and can be cured using conventional cure systems such as sulfur/sulfur donor or peroxides. Sufficient antioxidant is added during the manufacturing process for normal aging conditions.Highest ECH content terpolymer for improved heat and permeation resistance.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
Mooney Viscosity 80 - 100

@Temperature 100 °C
80 - 100

@Temperature 212 °F
(1+4)
Ash <= 1.0 %
<= 1.0 %
Zeon Test #1358
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -38.0 °C
-36.4 °F
Component Elements Properties Metric English Comments
Chlorine, Cl 28.1 - 30.1 %
28.1 - 30.1 %
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Zeon Test #1361
Descriptive Properties Value Comments
AGE Content, % 3.2-4.2