Zeon Chemicals Hydrin® T3106 Polyepichlorohydrin Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Hydrin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Hydrin® T3106 Polyepichlorohydrin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hydrin T3106 is an ethylene oxide/epichlorohydrin/allyl glycidyl ether terpolymer with high heat and solvent resistance. Compounds using Hydrin T3106 typically exhibit excellent low and high temperature properties and can be cured using conventional cure systems such as sulfur/sulfur donor or peroxides. Sufficient antioxidant is added during the manufacturing process for normal aging conditions.Highest EO content terpolymer for best low-temperature properties and enhanced electrostatic dissipative properties. Used in low-temperature hoses, air inlet ducts, and laser printer rolls.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
Mooney Viscosity 53 - 67

@Temperature 100 °C
53 - 67

@Temperature 212 °F
(1+4)
Ash <= 1.0 %
<= 1.0 %
Zeon Test #1358
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -48.0 °C
-54.4 °F
Component Elements Properties Metric English Comments
Chlorine, Cl 20.4 - 22.4 %
20.4 - 22.4 %
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Zeon Test #1361
Descriptive Properties Value Comments
AGE Content, % 5.9-7.9