Zeon Chemicals Nipol® DN4080 Nitrile Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Nipol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Nipol® DN4080 Nitrile Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nipol DN4080 is a copolymer of butadiene and acrylonitrile with very high oil resistance. Sufficient antioxidant is added during manufacture for normal storage conditions.Low mold fouling, fast curing and easy processing. High oil and fuel resistance.
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Mooney Viscosity 73 - 88

@Temperature 100 °C
73 - 88

@Temperature 212 °F
(1+4)
Ash <= 0.90 %
<= 0.90 %
Zeon Test #873
Descriptive Properties Value Comments
AO Type NS
Bound ACN (%, acrylonitrile) 38.5-41
Heat Loss (%) Max 0.8
Hot/Cold C