Zeon Chemicals Quintac® 3450 SIS Block Polymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Quintac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Quintac® 3450 SIS Block Polymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Styrene Isoprene (SIS) Block Polymer. Suitable for HMAInformation provided by Zeon Chemicals L.P.
Physical Properties Metric English Comments
Viscosity 240000 cP

@Temperature 180 °C
240000 cP

@Temperature 356 °F
Melt; Flowtester (100 kgf/cm², dimension of die 1 Φ mm x 10 mm)
Molecular Weight 200000 g/mol
200000 g/mol
Gel Permeation Chromatography
Melt Flow 16 g/10 min
16 g/10 min
Chemical Properties Metric English Comments
Styrene Content 19 %
19 %
Abbe's Refractometer
Diblock Content 30 %
30 %
Gel Permeation Chromatography