Material Notes:
PBZ-123 is a polyblend of hydrogenated nitrile polymer, Zetpol 1020, and polyvinyl chloride, Nippon Zeon 101EP. This material is mechanically fluxed to create a unique polyblend which exhibits good heat and sour gasoline resistance.Zetpol 1020 polyblend with PVC to provide an ideal material for fuel hoses and diaphragms.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
Iodine Absorption Number 20.3 - 28.5
20.3 - 28.5
mg/100mg; R-133A
Mooney Viscosity 118 - 132

@Temperature 100 °C
118 - 132

@Temperature 212 °F
(1+4); ZCI-T-003
Mechanical Properties Metric English Comments
Hardness, Shore A 75 - 85
75 - 85
R-351A
Tensile Strength at Break 19.61 - 39.22 MPa
2844 - 5688 psi
R-350A
Elongation at Break 350 - 600 %
350 - 600 %
R-350A
300% Modulus 0.01471 - 0.02941 GPa
2.133 - 4.266 ksi
R-350A
Descriptive Properties Value Comments
% HYD 91
Bound ACN (%, acrylonitrile) 27.4-30.5
Users viewing this material also viewed the following: