Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zotefoams ZOTEK® F 35 PVDF Foam

Category Polymer , Thermoplastic , Fluoropolymer , PVDF
Manufacturer Zotefoams
Trade Name ZOTEK®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zotefoams ZOTEK® F 35 PVDF Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Zotek® F 35 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.Information provided by Zotefoams
Physical Properties Metric English Comments
Density 0.0330 g/cc
0.00119 lb/in³
ISO 845
Water Absorption 0.060 %
0.060 %
ISO 2896
2.2 %
2.2 %
ASTM 1056
Cell Length 0.250 mm
0.00984 in
Mechanical Properties Metric English Comments
Tensile Strength 0.245 MPa
35.5 psi
ISO 1798
Elongation at Break 90 %
90 %
Compressive Yield Strength 0.0600 MPa

@Strain 25.0 %
8.70 psi

@Strain 25.0 %
ISO 7214
Tear Strength 0.700 kN/m
3.99 pli
ISO 8067
Compression Set 20 %

@Time 79200 sec,
Strain 50.0 %
20 %

@Time 22.0 hour,
Strain 50.0 %
0.5 hr recovery; ISO 7214
Thermal Properties Metric English Comments
Thermal Conductivity 0.0330 W/m-K
0.229 BTU-in/hr-ft²-°F
mean temp of 0°C; ISO 8301
0.0380 W/m-K
0.264 BTU-in/hr-ft²-°F
mean temp of 40°C; DIN 52 612
0.0460 W/m-K
0.319 BTU-in/hr-ft²-°F
mean temp of 80°C; ASTM C 518
Maximum Service Temperature, Air 110 °C
230 °F
Flammability, UL94 V-0
V-0