Zylog Hipolyene® 1703 MS HF Thermoplastic Polyolefin & PP Compound

Category Polymer , Thermoplastic , Polyolefin , Polypropylene (PP)
Manufacturer Zylog Plastalloys
Trade Name Hipolyene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zylog Hipolyene® 1703 MS HF Thermoplastic Polyolefin & PP Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
Melt Flow 18 g/10 min
18 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 9.81 MPa
1420 psi
Elongation at Break 250 %
250 %
Flexural Modulus 0.343 GPa
49.8 ksi