Information provided by Zylog Plastalloys Pvt. Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Melt Flow 18 g/10 min
18 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.6 MPa
3270 psi
Elongation at Break 30 %
30 %
Flexural Modulus 2.45 GPa
356 ksi
Izod Impact, Notched 0.981 J/cm
1.84 ft-lb/in