Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00200 cm/cm | 0.00200 in/in | ASTM D955 |
Niche Polymer PA6GF43BK Nylon 6, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00200 cm/cm | 0.00200 in/in | ASTM D955 |
Niche Polymer PA6GF43N Nylon 6, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00200 - 0.0130 cm/cm | 0.00200 - 0.0130 in/in | Average value: 0.00513 cm/cm Grade Count:5 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00404 cm/cm Grade Count:12 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00503 cm/cm Grade Count:58 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0450 cm/cm | 0.00200 - 0.0450 in/in | Average value: 0.00606 cm/cm Grade Count:250 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0114 cm/cm | 0.00200 - 0.0114 in/in | Average value: 0.00556 cm/cm Grade Count:81 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00537 cm/cm Grade Count:51 |
Overview of materials for Polystyrene, Transparent Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Transparent Grade". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0100 cm/cm | 0.00200 - 0.0100 in/in | Average value: 0.00671 cm/cm Grade Count:7 |
Overview of materials for Polyphenylene Ether, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00552 cm/cm Grade Count:106 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00700 cm/cm | 0.00200 - 0.00700 in/in | Average value: 0.00423 cm/cm Grade Count:15 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00700 cm/cm | 0.00200 - 0.00700 in/in | Average value: 0.00429 cm/cm Grade Count:14 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0200 cm/cm | 0.00200 - 0.0200 in/in | Average value: 0.0118 cm/cm Grade Count:15 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0120 cm/cm | 0.00200 - 0.0120 in/in | Average value: 0.00833 cm/cm Grade Count:10 |
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00950 cm/cm | 0.00200 - 0.00950 in/in | Average value: 0.00675 cm/cm Grade Count:4 |
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0250 cm/cm | 0.00200 - 0.0250 in/in | Average value: 0.0122 cm/cm Grade Count:10 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00400 cm/cm Grade Count:10 |
Overview of materials for Nylon 11 with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00400 cm/cm | 0.00200 - 0.00400 in/in | ASTM D955 |
Bhansali Engineering Abstron IM17SHG PMMA- ABS Alloy High GlossInformation provided by Bhansali |
|||
Linear Mold Shrinkage | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00400 cm/cm Grade Count:74 |
Overview of materials for Cellulose Acetate Propionate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Propionate, Molded". Each property range of values reported is minimum and maximum val.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00700 cm/cm | 0.00200 - 0.00700 in/in | Average value: 0.00369 cm/cm Grade Count:24 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00468 cm/cm Grade Count:11 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00500 cm/cm Grade Count:8 |
Overview of materials for Acrylic, UV Stabilized, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0150 cm/cm | 0.00200 - 0.0150 in/in | Average value: 0.00767 cm/cm Grade Count:13 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0400 cm/cm | 0.00200 - 0.0400 in/in | Average value: 0.0125 cm/cm Grade Count:44 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |