Physical Properties Metric English Comments
Linear Mold Shrinkage 0.000 - 0.0160 cm/cm
0.000 - 0.0160 in/in
Average value: 0.00232 cm/cm Grade Count:146
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Linear Mold Shrinkage 0.00500 - 0.0160 cm/cm
0.00500 - 0.0160 in/in
Average value: 0.00715 cm/cm Grade Count:53
Overview of materials for Polyphenylene Ether, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Molded". Each property range of values reported is minimum and maximum values of ap..
Linear Mold Shrinkage 0.00700 - 0.0160 cm/cm
0.00700 - 0.0160 in/in
Average value: 0.0108 cm/cm Grade Count:59
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be..
Linear Mold Shrinkage 0.000600 - 0.0160 cm/cm
0.000600 - 0.0160 in/in
Average value: 0.00542 cm/cm Grade Count:110
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Linear Mold Shrinkage 0.000200 - 0.0160 cm/cm
0.000200 - 0.0160 in/in
Average value: 0.00278 cm/cm Grade Count:82
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Linear Mold Shrinkage 0.00100 - 0.0160 cm/cm
0.00100 - 0.0160 in/in
Average value: 0.00409 cm/cm Grade Count:15
Overview of materials for Nylon 610, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage 0.00100 - 0.0160 cm/cm
0.00100 - 0.0160 in/in
Average value: 0.00673 cm/cm Grade Count:70
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..
Linear Mold Shrinkage 0.00200 - 0.0160 cm/cm
0.00200 - 0.0160 in/in
Average value: 0.00520 cm/cm Grade Count:7
Overview of materials for Polyphenylene Sulfide (PPS), Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Stainless Steel Fiber". Each property range of values reported is minimum a..
Linear Mold Shrinkage 0.000500 - 0.0160 cm/cm
0.000500 - 0.0160 in/in
Average value: 0.00227 cm/cm Grade Count:62
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi..
Linear Mold Shrinkage 0.000 - 0.0160 cm/cm
0.000 - 0.0160 in/in
Average value: 0.00477 cm/cm Grade Count:49
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Linear Mold Shrinkage 0.00800 - 0.0160 cm/cm
0.00800 - 0.0160 in/in
Average value: 0.0109 cm/cm Grade Count:14
Overview of materials for Polypropylene with 10% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are ..
Copyright © lookpolymers.com All Rights Reserved