Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.000100 - 0.0200 cm/cm | 0.000100 - 0.0200 in/in | ASTM D955 |
Niche Polymer PPHM15BK Homopolymer PP Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.00652 cm/cm Grade Count:92 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.00804 cm/cm Grade Count:75 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Linear Mold Shrinkage | 0.000 - 0.0200 cm/cm | 0.000 - 0.0200 in/in | Average value: 0.00468 cm/cm Grade Count:268 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Linear Mold Shrinkage | 0.000300 - 0.0200 cm/cm | 0.000300 - 0.0200 in/in | Average value: 0.00890 cm/cm Grade Count:21 |
Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage | 0.0000300 - 0.0200 cm/cm | 0.0000300 - 0.0200 in/in | Average value: 0.00889 cm/cm Grade Count:211 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Linear Mold Shrinkage | 0.0150 - 0.0200 cm/cm | 0.0150 - 0.0200 in/in | Average value: 0.0175 cm/cm Grade Count:3 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0200 cm/cm | 0.00200 - 0.0200 in/in | Average value: 0.00756 cm/cm Grade Count:17 |
Overview of materials for Silicone, RTV, Encapsulation Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value.. |
|||
Linear Mold Shrinkage | 0.00330 - 0.0200 cm/cm | 0.00330 - 0.0200 in/in | Average value: 0.0188 cm/cm Grade Count:24 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0200 cm/cm | 0.00200 - 0.0200 in/in | Average value: 0.0118 cm/cm Grade Count:15 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.00367 cm/cm Grade Count:47 |
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl.. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0200 cm/cm | 0.000500 - 0.0200 in/in | Average value: 0.00262 cm/cm Grade Count:50 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Linear Mold Shrinkage | 0.000300 - 0.0200 cm/cm | 0.000300 - 0.0200 in/in | Average value: 0.00496 cm/cm Grade Count:111 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.00494 cm/cm Grade Count:152 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.00995 cm/cm Grade Count:40 |
Overview of materials for Nylon 66, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu.. |
|||
Linear Mold Shrinkage | 0.000200 - 0.0200 cm/cm | 0.000200 - 0.0200 in/in | Average value: 0.00679 cm/cm Grade Count:284 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Linear Mold Shrinkage | 0.00700 - 0.0200 cm/cm | 0.00700 - 0.0200 in/in | Average value: 0.0142 cm/cm Grade Count:10 |
Overview of materials for Nylon 12, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.0200 cm/cm | 0.00400 - 0.0200 in/in | Average value: 0.0133 cm/cm Grade Count:29 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.00662 cm/cm Grade Count:38 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage | 0.00300 - 0.0200 cm/cm | 0.00300 - 0.0200 in/in | Average value: 0.00955 cm/cm Grade Count:136 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.0117 cm/cm Grade Count:27 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.00629 cm/cm Grade Count:115 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0200 cm/cm | 0.00100 - 0.0200 in/in | Average value: 0.00511 cm/cm Grade Count:287 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Linear Mold Shrinkage | 0.000600 - 0.0200 cm/cm | 0.000600 - 0.0200 in/in | Average value: 0.00418 cm/cm Grade Count:208 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0200 cm/cm | 0.0100 - 0.0200 in/in | Average value: 0.0146 cm/cm Grade Count:13 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.00150 - 0.0200 cm/cm | 0.00150 - 0.0200 in/in | Average value: 0.0119 cm/cm Grade Count:53 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |