Polymer Property : Linear Mold Shrinkage = 0.0220 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00200 - 0.0220 cm/cm
0.00200 - 0.0220 in/in
Average value: 0.0118 cm/cm Grade Count:101
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage 0.00100 - 0.0220 cm/cm
0.00100 - 0.0220 in/in
Average value: 0.00589 cm/cm Grade Count:58
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Linear Mold Shrinkage 0.0120 - 0.0220 cm/cm
0.0120 - 0.0220 in/in
Average value: 0.0176 cm/cm Grade Count:35
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m..
Linear Mold Shrinkage 0.000 - 0.0220 cm/cm
0.000 - 0.0220 in/in
Average value: 0.00607 cm/cm Grade Count:207
Overview of materials for Nylon 66, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Linear Mold Shrinkage 0.00500 - 0.0220 cm/cm
0.00500 - 0.0220 in/in
Average value: 0.0111 cm/cm Grade Count:15
Overview of materials for Nylon 66, Mineral Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v..