Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 64 SUS | 64 SUS | |
Lubriplate PM 500 White Oil USP Mineral -Based Food Machinery Grade This oil contains emulsifying agents that wet the lubricated surfaces and provide an oily film for the moving parts. Used very successfully on pear machines.Available in Bottles, Jugs, Pails, 1/4 Dr.. |