Polymer Property : Modulus of Elasticity = 10.79 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 1.70 - 10.79 GPa

@Temperature -100 - 200 °C
247 - 1565 ksi

@Temperature -148 - 392 °F
Average value: 4.65 GPa Grade Count:9
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..