Mechanical Properties Metric English Comments
Modulus of Elasticity 0.350 - 7.20 GPa

@Temperature 60.0 - 150 °C
50.8 - 1040 ksi

@Temperature 140 - 302 °F
Average value: 2.13 GPa Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
Modulus of Elasticity 0.350 GPa
50.8 ksi
ISO 527-2
Total Lacqtene® 1003 FE 30 HDPE, blow molding  (discontinued **)
Medium density radical polyethylene made by high tubular pressure process for medical applications requiring sterilization : small and medium stiff containers for parental mixtures, ophthalmic solut..
Modulus of Elasticity 0.350 - 0.840 GPa
50.8 - 122 ksi
Average value: 0.648 GPa Grade Count:7
Overview of materials for Medium Density Polyethylene (MDPE), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Molded". Each property range of values reported is minimum and maxim..
Modulus of Elasticity 0.350 - 1.90 GPa

@Temperature 60.0 - 150 °C
50.8 - 276 ksi

@Temperature 140 - 302 °F
Average value: 0.850 GPa Grade Count:1
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Modulus of Elasticity 0.350 - 2.23 GPa
50.8 - 323 ksi
Average value: 1.05 GPa Grade Count:34
Overview of materials for Nylon 12, Extrusion/Tubing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values ..
Modulus of Elasticity 0.350 GPa
50.8 ksi
ISO 5527
Total Lacqtene® 1008 FE 30 LDPE blown film  (discontinued **)
Low density radical polyethylene made by high pressure autoclave process. Grade for very stiff and transparent thin film. Applications examples: rigid bags, automatic packaging, thin shrink film.. A..
Modulus of Elasticity 0.350 - 3.50 GPa
50.8 - 508 ksi
Average value: 1.45 GPa Grade Count:44
Overview of materials for Nylon 6, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Modulus of Elasticity 0.350 - 13.0 GPa
50.8 - 1890 ksi
Average value: 2.29 GPa Grade Count:251
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..