Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 83.4 MPa @Strain 2.48 %, Temperature 23.0 °C |
12100 psi @Strain 2.48 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |