Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 0.339 - 4.51 J | 0.250 - 3.33 ft-lb | Average value: 1.02 J Grade Count:29 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |
|||
Gardner Impact | 0.339 - 4.52 J | 0.250 - 3.33 ft-lb | Average value: 0.693 J Grade Count:22 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |