Polymer Property : Four Ball Wear = 0.0209 in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Four Ball Wear 0.530 mm
0.0209 in
40 kg, 75°C, 1200 rpm; ASTM D4172
ExxonMobil Mobil Aero HFS
Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc..
Four Ball Wear 0.530 mm
0.0209 in
ChevronTexaco NLGI 1 Moly MAX Grease EP
FeaturesChevron Moly MAX Greases EP are high performance greases.They are formulated with extreme pressure additives and 5% molybdenum disulfide (moly). They are dark gray/black in color and smooth ..
Four Ball Wear 0.530 mm
0.0209 in
40 kg, 75°C, 1200 rpm; ASTM D4172
ExxonMobil Mobil Aero HFS
Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc..