Polymer Property : Film Tensile Strength at Break, MD = 136.96 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Film Tensile Strength at Break, MD 136.96 MPa
19865 psi
U2L98W; ASTM D882A
DuPont Teijin Films Teijin® Tetoron® U2 Polyester Film, 1000 Gauge
Teijin® Tetoron® U2 is an opaque white polyester film. Teijin® Tetoron® U2 is available in the following variants:U2: Non-pretreated; available in 150, 200, 300, 400, 500 & 1000 gaugeU298W: Adhe..