Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 20.7 - 48.0 MPa | 3000 - 6960 psi | Average value: 30.0 MPa Grade Count:7 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |
|||
Flexural Yield Strength | 21.0 - 48.0 MPa | 3050 - 6960 psi | Average value: 36.6 MPa Grade Count:10 |
Overview of materials for Polypropylene with 10% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are .. |