Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 961 MPa | 139000 psi | at Center, Transverse |
International Mold Steel PX5 Pre-Hardened Mold Steel (P20 Type) PX5 is a modified P20, high performance, high precision, mold steel. Unique Characteristics: Exceptionally clean steel with uniform microstructure – no pin holes, inclusions or hard spots. 30-3.. |
|||
Tensile Strength, Ultimate | 961 MPa | 139000 psi | at Center, Longitudinal |
International Mold Steel PX5 Pre-Hardened Mold Steel (P20 Type) PX5 is a modified P20, high performance, high precision, mold steel. Unique Characteristics: Exceptionally clean steel with uniform microstructure – no pin holes, inclusions or hard spots. 30-3.. |