Polymer Property : Tensile Strength, Ultimate = 12500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.0 - 86.0 MPa
9430 - 12500 psi
Average value: 80.4 MPa Grade Count:7
Overview of materials for Nylon 6, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate..
Tensile Strength, Ultimate 53.4 - 86.0 MPa
7750 - 12500 psi
Average value: 66.8 MPa Grade Count:5
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum..