Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 0.517 MPa

@Time 900 sec
75.0 psi

@Time 0.250 hour
Overlap of Build-Up, 1/8 birch to 1/8 birch, 25°C at 50% RH Aged; ASTM D1002
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1
3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced..
Shear Strength 0.517 MPa

@Time 900 sec
75.0 psi

@Time 0.250 hour
Overlap of Build-Up, 1/8 birch to 1/8 birch, 32°C at 90% RH Aged; ASTM D1002
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1
3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced..
Shear Strength 0.517 MPa

@Temperature 82.0 °C
75.0 psi

@Temperature 180 °F
1/8" Birch/High-Pressure Laminate, aged 6 mo
3M Fastbond™ 30-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M
Shear Strength 0.517 MPa

@Temperature 82.0 °C
75.0 psi

@Temperature 180 °F
1/8" Birch/High-Pressure Laminate, aged 6 mo
3M Fastbond™ 30H-NF Contact Adhesive
3M Fastbond™ Contact Adhesive 30-NF and 30H-NF are water-dispersed, sprayable contact adhesives for high immediate bond strength n long bonding range.Information provided by 3M