Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 82.0 °C | 180 °F | ISO 306/A50 |
Premix Thermoplastics PRE-ELEC® ESD 6600 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 6000 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6000 has b.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Geloy XTWE270M ASA+SAN (Asia Pacific) Excellent weatherability, good flow/aesthetics and good impact.Profile co-extrusion grade over ABS, PVC or other compatible polymers. XTWE270M is available in various colours.This data was supplied.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ISO 306 |
Polycasa LENTICULAR PETG Good ink adhesionGood receptabilityStable sheet dimensionsHigh impact strengthGood chemical resistanceEnvironmentally safeRecyclableMeets current food contact legislationDisplays Graphic Arts Advert.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | DIN 53460 |
Polycasa PETG QUINN PETG has good optical properties and a brilliant surface. The PETG range of sheets are easy to fabricate, to vacuum form, and show exceptional low temperature performance. Important benefits o.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1252 |
Total Finaclear® 530 Clear Impact Polystyrene
(discontinued **) Finaclear® 530 is a clear high styrenic styrene-butadiene (SBS) elastomer, providing dramatically improved impact properties and tear resistance to finished articles, when used in blends with other.. |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RK 325/AM Rigid PVC, Extrusion Lead Free Profiles anti mould |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RK 435 Rigid PVC, Extrusion Lead Free Electrical channels |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
LyondellBasell Plexar® PX3227 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ISO 306B |
Lucite International Diakon® ST45G6 Toughened Acrylic Polymer The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ISO 306 |
Iran Petrochemical (PCC) 1922T Low Density Polyethylene LDPE 1922T - for injection molding with a balance between flow properties and mechanical propertiesApplications: toys, household articles, clamping lids.Information provided by Iran Petrochemical Co.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ISO 306 |
Stir SpA HE 625 A (PVC) Application: Economic medium shock resistantInformation provided by STIR SpA |
|||
Vicat Softening Point | 82.0 °C | 180 °F | VST/B/50; ISO 306 |
Styrolution Polystyrol 454 C GR 2 PS Description: Polystyrol 454 C is an impact resistant polystyrene with a good balance of toughness, high flow, heat resistance and high gloss.Applications: TV-front panels and back covers, VCR fronts.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
SK Chemicals SKYTHANE® 180A R series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
DuPont Elvax® 3135X Ethylene-Vinyl Acetate Copolymer Resin for Thin Blown 12 wt% Vinyl Acetate.Elvax® 3135X is an extrudable, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resi.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525, ISO 306 |
DuPont Elvax® 3135XZ Ethylene Vinyl Acetate DuPont™ Elvax® 3135XZ is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.Applicati.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ISO 306 |
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film EVA 1010 VN 3 is made by a high pressure tubular process. Grade for films with high transparency and high mechanical properties. Contains an antioxidant.Application examples: Stretch film, food pa.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525 |
DuPont Bynel® 3930 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525, ISO 306 |
DuPont™ Bynel® 41E865 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds R 316 Rigid PVC, Extrusion Rolling shutters |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds R 316/AS Rigid PVC, Extrusion Antistatic profiles |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 121 Rigid PVC, Extrusion Electric pipes |
|||
Vicat Softening Point | 82.0 °C | 180 °F | 50N (T° increase = 5°C/h); ISO 306B50 |
Total Lacqrene® 6630 Impact Polystyrene
(discontinued **) LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application.. |
|||
Vicat Softening Point | 82.0 °C | 180 °F | 1000g; ASTM D-1525 |
ExxonMobil Escorene® LD-712 High EVA Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt, 10% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness... |
|||
Vicat Softening Point | 82.0 - 84.0 °C @Load 5.00 kg |
180 - 183 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RE 230/D Rigid PVC, Extrusion Electric channels |
|||
Vicat Softening Point | 82.0 °C | 180 °F | ASTM D1525, ISO 306 |
DuPont Elvax® 880 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 880 is an ethylene-vinyl acetate copolymer resin containing slip and anti-block additives for use in industrial applications.Applications: Elvax® 880 resins can be used for the fo.. |