Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 198 °C | 388 °F | ISO METHOD 3146C |
NYCOA 2061 Copolymer Nylon 6/69 monofilament weed eater, fishing lineInformation provided by NYCOA, Inc. |
|||
Melting Point | 198 - 208 °C | 388 - 406 °F | Temperature range at which MFI = 10 g/10 min at 21.6 kg.; MQSA 111 |
Lubrizol Advanced Materials Pearlthane® 11T75D Thermoplastic Polyurethane Elastomer Pearlthane® 11T75D is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, with extremely high hardness. It is especially recommended for use in producin.. |
|||
Melting Point | <= 198 °C | <= 388 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 00014 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00014 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic.. |