Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 198 - 208 °C | 388 - 406 °F | Temperature range at which MFI = 10 g/10 min at 21.6 kg.; MQSA 111 |
Lubrizol Advanced Materials Pearlthane® 11T75D Thermoplastic Polyurethane Elastomer Pearlthane® 11T75D is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, with extremely high hardness. It is especially recommended for use in producin.. |