Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.00 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.89 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott WG305 Long Pass Filter Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66.. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 - 300 °C |
3.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-BAF10 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature -30.0 - 70.0 °C |
3.89 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-BAK4 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 - 300 °C |
3.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LAF34 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 - 300 °C |
3.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LAK33A Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 - 400 °C |
3.89 µin/in-°F @Temperature 68.0 - 752 °F |
DIN EN 821-1 |
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2 DN 70 is a ZTA Alumina Toughened Zirconia. |
|||
CTE, linear | 7.00 - 9.00 µm/m-°C @Temperature 20.0 - 600 °C |
3.89 - 5.00 µin/in-°F @Temperature 68.0 - 1110 °F |
ASTM-C373 |
CeramTec Frequenta® Steatite Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. Frequenta® has low dielectric loss, but has be.. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 - 600 °C |
3.89 µin/in-°F @Temperature 68.0 - 1110 °F |
ASTM-C372 |
CeramTec Rubalit® 702 Alumina, 85% Rubalit® 702 is a high-performance material for the manufacturing of metal-film resistors. With an alumina content of 85%, it provides extreme hardness and high thermal conductivity. Practical appl.. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 25.0 - 300 °C |
3.89 µin/in-°F @Temperature 77.0 - 572 °F |
ASTM-C372 |
CoorsTek ADS-995 99.5% Alumina Thin Film Applications: thin film substrates |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 25.0 - 300 °C |
3.89 µin/in-°F @Temperature 77.0 - 572 °F |
ASTM-C372 |
CoorsTek ADS-996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 25.0 - 300 °C |
3.89 µin/in-°F @Temperature 77.0 - 572 °F |
ASTM-C372 |
CoorsTek Superstrate® 996 99.6% Alumina Thin Film Applications: thin film substrates |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 30.0 - 400 °C |
3.89 µin/in-°F @Temperature 86.0 - 752 °F |
|
Ametek Molybdenum-Copper Composite AMC 8515 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 20.0 - 400 °C |
3.89 µin/in-°F @Temperature 68.0 - 752 °F |
|
Assab Steels QRO 90 SUPREME Hot Work Steel QRO 90 SUPREME is a high-performance, chromium-molybdenum-vanadium alloyed hot-work tool steel which is characterized by: Excellent high temperature strength and hot hardnessVery good temper resista.. |
|||
CTE, linear | 7.00 µm/m-°C @Temperature 30.0 - 400 °C |
3.89 µin/in-°F @Temperature 86.0 - 752 °F |
|
Ametek Tungsten-Copper Composites AWC 8812 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |