Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -118 - 82.2 °C | -180 - 180 °F | Average value: -82.3 °C Grade Count:137 |
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum.. |