Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1.40e+15 ohm-cm | 1.40e+15 ohm-cm | ASTM D257 |
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Electrical Resistivity | 1.40e+15 - 2.70e+15 ohm-cm @Temperature 90.0 - 90.0 °C |
1.40e+15 - 2.70e+15 ohm-cm @Temperature 194 - 194 °F |
Average value: 2.27e+15 ohm-cm Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |