Electrical Properties Metric English Comments
Dielectric Strength 3.50 kV/mm
88.9 kV/in
ASTM D150
Rogers Corporation Bisco™ BF-1000 Cellular Silicone Foam
Soft, low compression set silicone foam often specified to meet safely-conscious requirements. UL recognized for flame retardance.Applications: Low closure-force gaskets and seals, Vibration and sh..
Dielectric Strength 3.50 kV/mm
88.9 kV/in
ASTM D150
Rogers Corporation Bisco™ HT-870 Cellular Silicone Foam
Gasketing and sealing rating is JMLU-2 (Listed) per UL 157. No UV degradation per SAE J-1960. Ozone effect rating is 0 (no cracks) per ASTM D-1171. No staining per ASTM D-925(A). Passes AMS-3568..
Dielectric Strength 3.50 - 7.48 kV/mm
88.9 - 190 kV/in
Average value: 4.71 kV/mm Grade Count:7
Overview of materials for Silicone Foam
This property data is a summary of similar materials in the MatWeb database for the category "Silicone Foam". Each property range of values reported is minimum and maximum values of appropriate MatW..
Dielectric Strength 3.50 kV/mm
88.9 kV/in
ASTM D149
3M Dyneon™ 1750 PTFE Powder  (discontinued **)
Type II PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r..
Dielectric Strength 3.50 kV/mm
88.9 kV/in
150°C for 1,000 hrs
Fujipoly Industries Sarcon® 15GTR Thin-Film GTR
Sarcon TR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GTR is a composite of ..
Dielectric Strength 3.50 kV/mm

@Thickness 3.00 mm
88.9 kV/in

@Thickness 0.118 in
24hr/23°C/50% RH+1hr/oil 90°C; Perpendicular; IEC 60243-1; IEC/EN 61212-2 6.1.2.1
Elektro-Isola Etronit B67 Phenolic, Paper Reinforcement, Dark Brown, Tubes
Description: For mechanical and electrical low-voltage applications. Very good electrical properties at high air humidity. Applications: Winding tubes in the foil and metal foil industries and carri..
Dielectric Strength 3.50 - 5.00 kV/mm

@Temperature 90.0 °C
88.9 - 127 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATG 112 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic ..
Dielectric Strength >= 3.50 kV/mm
>= 88.9 kV/in
disk; ASTM D877
Paratherm Corporation Paratherm™ OR Heat Transfer Fluid
Description: Paratherm OR® is a sludge-resistant heat transfer fluid that combines substantial oxidation resistance with excellent thermal efficiency, high flash and fire points and extended servic..
Copyright © lookpolymers.com All Rights Reserved