Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Manufacturer : LATI > Category : Thermoplastic Product List

Tips:Up to 100 items are displayed.
PRODUCT NO. Category Trade Name
LATI Kelon® B FR H2 CE/25-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Nylon 6 Kelon® B
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Nylon 6, Glass/Mineral Reinforced Kelon® B
LATI Kelon® B H CER/30 PA 6, 30% Mineral Reinforced, Heat Stabilized Nylon 6, 30% Mineral Filled Kelon® B
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant Polyphthalamide (PPA), 30% Glass Fiber Reinforced Laramid
LATI Laramid G/35 PPA, 35% Glass Fiber Reinforced Polyphthalamide (PPA), 40% Glass Fiber Reinforced Laramid
LATI Laramid G/45 PPA, 45% Glass Fiber Reinforced Polyphthalamide (PPA), 50% Glass Fiber Reinforced Laramid
LATI Laramid G/50 PPA, 50% Glass Fiber Reinforced Polyphthalamide (PPA), 50% Glass Fiber Reinforced Laramid
LATI Laril 13-V1KC PPOm, Mineral Reinforced, Flame Retardant Polyphenylene Ether, Mineral Filled Laril
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced Polyetheretherketone, PEEK, Glass Fiber Filled Larpeek
LATI Larpeek 10 GCE/600 PEEK, Glass/Mineral Reinforced Polyetheretherketone, PEEK, Glass Fiber Filled Larpeek
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone, PEEK, Carbon Fiber Filled Larpeek
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone, PEEK, Carbon Fiber Filled Larpeek
LATI Larpeek 10 PEEK Polyetheretherketone, PEEK, Unreinforced Larpeek
LATI Larpeek 50 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone, PEEK, Glass Fiber Filled Larpeek
LATI Larpeek 50 K/30 PEEK, 30% Carbon Fiber Reinforced Polyetheretherketone, PEEK, Carbon Fiber Filled Larpeek
LATI Larpeek 50 PEEK Polyetheretherketone, PEEK, Unreinforced Larpeek
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler Larton
LATI Larton GCE/600 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled Larton
LATI Larton GCE/650 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled Larton
LATI Larton GK/400 PPS, Glass/Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) Larton
LATI Larton K/20 PPS, 20% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler Larton
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced Polyphenylene Sulfide (PPS) with 40% Carbon Fiber Filler Larton
LATI Larton L G/40 L-PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler Larton
LATI Larton MDT16-02 PPS Polyphenylene Sulfide (PPS) Larton
LATI Lastane 50 PUR Polyurethane, TP Lastane
LATI Lastil G/25-V0 SAN, 25% Glass Fiber Reinforced, Flame Retardant Styrene Acrylonitrile (SAN), Molded, Glass Reinforced Lastil
LATI Lastilac 10 ABS/PC Polycarbonate/ABS Alloy, Unreinforced Lastilac
LATI Lastilac AR G/17-V0E ABS, 17% Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled Lastilac
LATI Lastilac RT K/10 ABS, 10% Carbon Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled Lastilac
LATI Lastilac SP G/17 ABS, Glass Fiber Reinforced Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled Lastilac
LATI Lasulf G/15 PSU, 15% Glass Fiber Reinforced Polysulfone, 20% Glass Fiber Reinforced Lasulf
LATI Lasulf G/20 PSU, 20% Glass Fiber Reinforced Polysulfone, 20% Glass Fiber Reinforced Lasulf
LATI Lasulf PSU Polysulfone (PSU) Lasulf
LATI Latamid 12 CP/85 PA 12 Nylon 12 Latamid
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced Nylon 12, 50% Glass Fiber Filled Latamid
LATI Latamid 12 H FE90 PA 12, Heat Stabilized Nylon 12 Latamid
LATI Latamid 12 H2 K/30 PA 12, 30% Carbon Fiber Reinforced, Heat Stabilized Nylon 12, 30% Glass Fiber Filled Latamid
LATI Latamid 6 E02 PA 6, Impact modified Nylon 6, Impact Grade Latamid
LATI Latamid 6 H2 G/20-V0 PA 6, 20% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Nylon 6, Glass Fiber Filled, Flame Retardant Latamid
LATI Latamid 6 H2 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized Nylon 6, 30% Glass Fiber Filled Latamid
LATI Latamid 6 H2 G/30-V0CT1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Nylon 6, Glass Fiber Filled, Flame Retardant Latamid
LATI Latamid 6 H2 G/30-V0HF1 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Nylon 6, Glass Fiber Filled, Flame Retardant Latamid
LATI Latamid 6 H2 G/35 PA 6, 35% Glass Fiber Reinforced, Heat Stabilized Nylon 6, 40% Glass Fiber Filled Latamid
LATI Latamid 6 H2 G/55 PA 6, 55% Glass Fiber Reinforced, Heat Stabilized Nylon 6, 60% Glass Fiber Filled Latamid
LATI Latamid 6 H2E04 G/30 PA 6, 30% Glass Fiber Reinforced, Heat Stabilized Nylon 6, 30% Glass Fiber Filled Latamid
LATI Latamid 6 H-V0 PA 6, Heat Stabilized, Flame Retardant Nylon 6, Unreinforced, Flame Retardant Latamid
LATI Latamid 66 B H-V0 PA 66, Heat Stabilized, Flame Retardant Nylon 66, Unreinforced, Flame Retardant Latamid
LATI Latamid 66 E21 G/15 PA 66, 15% Glass Fiber Reinforced Nylon 66, 20% Glass Fiber Filled Latamid
LATI Latamid 66 E21 K/30 PA 66, 30% Carbon Fiber Reinforced Nylon 66, 30% Carbon Fiber Filled Latamid
LATI Latamid 66 E21 PA 66, Impact Modified Nylon 66, Impact Grade Latamid
LATI Latamid 66 H2 G/35-V0KB PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Nylon 66, 40% Glass Fiber Filled Latamid
LATI Latamid 66 H2 G/35-V0KB1 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Nylon 66, 40% Glass Fiber Filled Latamid
LATI Latamid 66 H2 G/35-V0KB3 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Nylon 66, 40% Glass Fiber Filled Latamid
LATI Latamid 66 H2 G/50 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized Nylon 66, 50% Glass Fiber Filled Latamid
LATI Latamid 66 H2 G/50-GWHF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized Nylon 66, 50% Glass Fiber Filled Latamid
LATI Latamid 66 H2 G/50-V0HF1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Nylon 66, 50% Glass Fiber Filled Latamid
LATI Latamid 66 H2 G/50-V0KB1 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized, Flame Retardant Nylon 66, 50% Glass Fiber Filled Latamid
LATI Latamid 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized Nylon 66, 60% Glass Fiber Filled Latamid
LATI Latamid 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized Nylon 66, 30% Carbon Fiber Filled Latamid
LATI Latamid 66 H2 K/40 PA 66, 40% Carbon Fiber Reinforced, Heat Stabilized Nylon 66, 40% Carbon Fiber Filled Latamid
LATI Latamid 66 H2 K/50 PA 66, 50% Carbon Fiber Reinforced, Heat Stabilized Nylon 66, 50% Carbon Fiber Filled Latamid
LATI Latamid 66 H2E21 G/13 PA 66, 13% Glass Fiber Reinforced Nylon 66, 10% Glass Fiber Filled Latamid
LATI Latamid 66 H2PX-V0 PA 66, Heat Stabilized, Flame Retardant Nylon 66, Unreinforced, Flame Retardant Latamid
LATI Latamid 66 H-V0 PA 66, Heat Stabilized, Flame Retardant Nylon 66, Unreinforced, Flame Retardant Latamid
LATI Latamid 66 LH2 G/35 PA 66, 35% Glass Fiber Reinforced, Heat Stabilized Nylon 66, Heat Stabilized Latamid
LATI Latamid 66 MDT03-01 PA 66 Nylon 66 Latamid
LATI Latamid 66 MDT05-01 PA 66 Nylon 66 Latamid
LATI Latamid 66 PA 66 Nylon 66, Unreinforced Latamid
LATI Latamid 66 VH2 G/30 PA 66, 30% Glass Fiber Reinforced Nylon 66, 30% Glass Fiber Filled Latamid
LATI Latamid SP1 G/30 PA 6.10, 30% Glass Fiber Reinforced Nylon 610, Glass Reinforced Latamid
LATI Latene® 7H2W TR/40 PP Homopolymer, Mineral Reinforced, Heat Stabilized Polypropylene, Mineral Reinforced Latene®
LATI Latene® 7H2W T-V0 PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant Polypropylene, Flame Retardant Latene®
LATI Latene® 7H2W T-V0E PP Homopolymer, Mineral Reinforced, Heat Stabilized, Flame Retardant Polypropylene, Flame Retardant Latene®
LATI Latene® 7H2W-V0 PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene, Flame Retardant Latene®
LATI Latene® 7-V2 PP Homopolymer, Flame Retardant Polypropylene, Flame Retardant Latene®
LATI Kelon® B FR H CET/05-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Nylon 6 Kelon® B
LATI Kelon® B FR H CET/30-V0 PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Nylon 6 Kelon® B
LATI Kelon® B FR H CETG/250-V0 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Nylon 6, Glass/Mineral Reinforced Kelon® B
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized Nylon 6, 30% Mineral Filled Kelon® B
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized Nylon 6, Glass/Mineral Reinforced Kelon® B
LATI Lapex A G/10 PES, 10% Glass Fiber Reinforced Polyethersulfone (PES), 10%Glass Fiber Filled Lapex
LATI Lapex A G/20 PES, 20% Glass Fiber Reinforced Polyethersulfone (PES), 20%Glass Fiber Filled Lapex
LATI Lapex A PES Polyethersulfone (PES) Lapex
LATI Lapex R G/10 PPSU, 10% Glass Reinforced Polyphenylsulfone (PPSU) Lapex
LATI Lapex R G/20 PPSU, 20% Glass Reinforced Polyphenylsulfone (PPSU) Lapex
LATI Lapex R PPSU Polyphenylsulfone (PPSU) Lapex
LATI Laramid CE/60 PPA, 60% Mineral Reinforced Polyphthalamide (PPA), Mineral Filled Laramid
LATI Laramid G/15 PPA, 15% Glass Fiber Reinforced Polyphthalamide (PPA), 20% Glass Fiber Reinforced Laramid
LATI Laramid G/30 PPA, 30% Glass Fiber Reinforced Polyphthalamide (PPA), 30% Glass Fiber Reinforced Laramid
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced Polyphthalamide (PPA) Laramid
LATI Laramid K/40 HM PPA, 40% Carbon Fiber Reinforced Polyphthalamide (PPA), Carbon Fiber Filled Laramid
LATI Laril 13 G/10-V1 PPOm, 10% Glass Fiber Reinforced, Flame Retardant Polyphenylene Ether, 10% Glass Filled Laril
LATI Laril 13 G/20 PPOm, 20% Glass Fiber Reinforced Polyphenylene Ether, 20% Glass Filled Laril
LATI Laril 13 G/20-V1 PPOm, 20% Glass Fiber Reinforced, Flame Retardant Polyphenylene Ether, 20% Glass Filled Laril
LATI Laril 13 G/30 PPOm, 30% Glass Fiber Reinforced Polyphenylene Ether, 30% Glass Filled Laril
LATI Laril 13 G/30-V1 PPOm, 30% Glass Fiber Reinforced, Flame Retardant Polyphenylene Ether, 30% Glass Filled Laril
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced Polyetheretherketone, PEEK, Glass Fiber Filled Larpeek
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced Polyetheretherketone, PEEK, Glass Fiber Filled Larpeek
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced Polyetheretherketone, PEEK, Glass Fiber Filled Larpeek
LATI Larpeek 10 G/60 PEEK, 60% Glass Fiber Reinforced Polyetheretherketone, PEEK, Glass Fiber Filled Larpeek
Copyright © lookpolymers.com All Rights Reserved