PRODUCT NO. Category Trade Name
Lucent Polymers 6-01 Nylon 6, General Purpose, Injection Grade Nylon 6
Lucent Polymers 66-01 Nylon 66, General Purpose, Injection Grade Nylon 66
Lucent Polymers 66-41 Nylon 66, Toughened Nylon 66, Impact Grade
Lucent Polymers ABS-305 Acrylonitrile Butadiene Styrene, General Purpose ABS Polymer
Lucent Polymers ABS-305LG Acrylonitrile Butadiene Styrene, General Purpose, Low Gloss ABS Polymer
Lucent Polymers ABS-45T Acrylonitrile Butadiene Styrene, High Impact Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Lucent Polymers CPP-0107 Polypropylene Homopolymer Renewable/Recycled Polymer
Lucent Polymers CPP-0307 Polypropylene, Mineral Filled, Impact Modified Renewable/Recycled Polymer
Lucent Polymers CPP-110 Polypropylene Homopolymer, 10% Calcium Carbonate Filled Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
Lucent Polymers CPP-120 Polypropylene Homopolymer, 20% Calcium Carbonate Filled Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Lucent Polymers CPP-130 Polypropylene Homopolymer, 30% Calcium Carbonate Filled Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
Lucent Polymers CPP-140 Polypropylene Homopolymer, 40% Calcium Carbonate Filled Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Lucent Polymers CPP-210 Polypropylene, 10% Calcium Carbonate Filled, Impact Modified Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
Lucent Polymers CPP-220 Polypropylene, 20% Calcium Carbonate Filled, Impact Modified Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Lucent Polymers CPP-230 Polypropylene, 30% Calcium Carbonate Filled, Impact Modified Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
Lucent Polymers CPP-240 Polypropylene, 40% Calcium Carbonate Filled, Impact Modified Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Lucent Polymers CPP-310 Polypropylene, 10% Calcium Carbonate Filled, Impact Modified Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
Lucent Polymers CPP-320 Polypropylene, 20% Calcium Carbonate Filled, Impact Modified Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Lucent Polymers CPP-330 Polypropylene, 30% Calcium Carbonate Filled, Impact Modified Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
Lucent Polymers CPP-340 Polypropylene, 40% Calcium Carbonate Filled, Impact Modified Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Lucent Polymers G6-15 Nylon 6, 15% Glass Fiber Reinforced Nylon 6, 20% Glass Fiber Filled
Lucent Polymers G6-33 Nylon 6, 33% Glass Fiber Reinforced Nylon 6, 30% Glass Fiber Filled
Lucent Polymers G66-13 Nylon 66, 13% Glass Fiber Reinforced Nylon 66, 10% Glass Fiber Filled
Lucent Polymers G66-33 Nylon 66, 33% Glass Fiber Reinforced Nylon 66, 30% Glass Fiber Filled
Lucent Polymers GPB-115 Polybutylene Terephthalate, 15% Glass Fiber Reinforced Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
Lucent Polymers GPB-130 Polybutylene Terephthalate, 30% Glass Fiber Reinforced Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Lucent Polymers GPB-130L Polybutylene Terephthalate, 30% Glass Fiber Reinforced Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Lucent Polymers GPB-FR515 Polybutylene Terephthalate, 15% Glass Fiber Reinforced, Flame Resistant Polybutylene Terephthalate (PBT), Flame Retardant
Lucent Polymers GPC-0202 20 Polycarbonate, Glass Reinforced, Injection Grade Polycarbonate, 20% Glass Filled
Lucent Polymers GPCB-110 Polycarbonate+PBT, 10% Glass Fiber Reinforced Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
Lucent Polymers GPCB-120 Polycarbonate+PBT, 20% Glass Fiber Reinforced Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
Lucent Polymers GPCB-330 Polycarbonate+PBT, 30% Glass Fiber Reinforced, Impact Resistant Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
Lucent Polymers GPP-110 Polypropylene Homopolymer, 10% Glass Fiber Reinforced, Chemically Coupled Polypropylene with 10% Glass Fiber Filler
Lucent Polymers GPP-120 Polypropylene Homopolymer, 20% Glass Fiber Reinforced, Chemically Coupled Polypropylene with 20% Glass Fiber Filler
Lucent Polymers GPP-130 Polypropylene Homopolymer, 30% Glass Fiber Reinforced, Chemically Coupled Polypropylene with 30% Glass Fiber Filler
Lucent Polymers GPP-140 Polypropylene Homopolymer, 40% Glass Fiber Reinforced, Chemically Coupled Polypropylene with 40% Glass Fiber Filler
Lucent Polymers GPP-210 Polypropylene, 10% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Polypropylene with 10% Glass Fiber Filler
Lucent Polymers GPP-220 Polypropylene, 20% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Polypropylene with 20% Glass Fiber Filler
Lucent Polymers GPP-230 Polypropylene, 30% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Polypropylene with 30% Glass Fiber Filler
Lucent Polymers GPP-240 Homopolymer Polypropylene, 40% Glass Fiber Reinforced, Chemically Coupled Polypropylene with 40% Glass Fiber Filler
Lucent Polymers GPP-310 Polypropylene, 10% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Polypropylene with 10% Glass Fiber Filler
Lucent Polymers GPP-320 Polypropylene, 20% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Polypropylene with 20% Glass Fiber Filler
Lucent Polymers GPP-330 Polypropylene, 30% Glass Fiber Reinforced, Chemically Coupled, Impact Modified Polypropylene with 30% Glass Fiber Filler
Lucent Polymers GPP-340 Polypropylene Homopolymer, 40% Glass Fiber Reinforced, Chemically Coupled Polypropylene with 40% Glass Fiber Filler
Lucent Polymers L6-140 Nylon 6, 15% Glass Fiber and 25% Mineral Reinforced Nylon 6, 30% Mineral Filled
Lucent Polymers LPB-130 Polybutylene Terephthalate, 30% Glass Fiber/Mineral Reinforced, Low Warp Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Lucent Polymers PBT-310 Polybutylene Terephthalate, 30% Glass Fiber/Mineral Reinforced, Low Warp Polybutylene Terephthalate (PBT), Glass + Mineral Filled
Lucent Polymers PBT-FR310 Polybutylene Terephthalate, Flame Resistant Polybutylene Terephthalate (PBT), Flame Retardant
Lucent Polymers PC/ABS-0406 Polycarbonate+ABS, Injection Grade Polycarbonate/ABS Alloy, Unreinforced
Lucent Polymers PC/ABS-1003 Polycarbonate+ABS, Extrusion / General Purpose, Injection Grade Polycarbonate/ABS Alloy, Unreinforced
Lucent Polymers PC/ABS-1020 Polycarbonate+ABS, General Purpose, Injection Grade Polycarbonate/ABS Alloy, Unreinforced
Lucent Polymers PC/ABS-1208 Polycarbonate+ABS, General Purpose, Injection Grade Polycarbonate/ABS Alloy, Unreinforced
Lucent Polymers PC/ABS-1211P Polycarbonate+ABS, Impact Modified, Platable, Injection Grade Polycarbonate/ABS Alloy, Unreinforced
Lucent Polymers PC/ABS-1216LG Polycarbonate+ABS, Low Gloss, Injection Grade Polycarbonate/ABS Alloy, Unreinforced
Lucent Polymers PC/ABS-1218 Polycarbonate+ABS, Easy Flow, Injection Grade Polycarbonate/ABS Alloy, Unreinforced
Lucent Polymers PC/ABS-FR0 Polycarbonate+ABS, Flame Resistant Polycarbonate/ABS Alloy, Unreinforced
Lucent Polymers PC/PBT-0820 Polycarbonate+PBT, Injection Grade Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Lucent Polymers PC/PBT-1020 Polycarbonate+PBT, General Purpose, Injection Grade Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Lucent Polymers PC/PBT-1212 Polycarbonate+PBT, General Purpose, Injection Grade Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Lucent Polymers PC/PBT-1230 Polycarbonate+PBT, General Purpose, Injection Grade Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Lucent Polymers PC/PBT-1231 Polycarbonate+PBT, General Purpose, Injection Grade Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Lucent Polymers PC/PBT-1420IM Polycarbonate+PBT, Superior Cold Temp Impact, Injection Grade Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Lucent Polymers PC/PBT-1422 Polycarbonate+PBT, Improved Cold Temp Impact, Injection Grade Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Lucent Polymers PC/PBT-1430U Polycarbonate+PBT, Superior Weatherability, Injection Grade Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Lucent Polymers PC/PBT-1550 Polycarbonate+PBT, Improved Impact Resistance, Injection Grade Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Lucent Polymers PC/PBT-1830 Polycarbonate+PBT, Superior Cold Temp Impact, Injection Grade Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
Lucent Polymers PC/PET-1515 Polycarbonate+PET, General Purpose, Injection Grade Polycarbonate/PET Polyester Blend
Lucent Polymers PC-1403 Polycarbonate, Extrusion/Blow Molding Grade Polycarbonate (PC)
Lucent Polymers PC-1403FD Polycarbonate, FDA Compliant, Extrusion/Blow Molding Grade Polycarbonate (PC)
Lucent Polymers PC-1406 Polycarbonate, Extrusion/Blow Molding Grade Polycarbonate (PC)
Lucent Polymers PC-1406FD Polycarbonate, FDA Compliant, Extrusion/Blow Molding Grade Polycarbonate (PC)
Lucent Polymers PC-1410 Polycarbonate, Injection/Extrusion Grade Polycarbonate (PC)
Lucent Polymers PC-1410FD Polycarbonate, FDA Compliant, Injection/Extrusion Grade Polycarbonate (PC)
Lucent Polymers PC-1418 Polycarbonate, Injection Grade Polycarbonate (PC)
Lucent Polymers PC-1418FD Polycarbonate, FDA Compliant, Injection Grade Polycarbonate (PC)
Lucent Polymers PC-1425 Polycarbonate, Injection Grade Polycarbonate (PC)
Lucent Polymers PC-1428 Polycarbonate, Injection Grade Polycarbonate (PC)
Lucent Polymers PC-1428FD Polycarbonate, FDA Compliant, Injection Grade Polycarbonate (PC)
Lucent Polymers PC-FR0 Polycarbonate, Flame Resistant Polycarbonate, Unreinforced, Flame Retardant
Lucent Polymers PC-FR2 Polycarbonate, Flame Resistant Polycarbonate, Unreinforced, Flame Retardant
Lucent Polymers TPO-20T Thermoplastic Polyolefin, 20% Mineral Filled Polyolefin
Lucent Polymers TPO-30T Thermoplastic Polyolefin, 30% Mineral Filled Polyolefin
Lucent Polymers TPP-110 Polypropylene, Homopolymer, 10% Talc Filled Polypropylene with 10% Talc Filler
Lucent Polymers TPP-120 Polypropylene, Homopolymer, 20% Talc Filled Polypropylene with 20% Talc Filler
Lucent Polymers TPP-130 Polypropylene, Homopolymer, 30% Talc Filled Polypropylene with 30% Talc Filler
Lucent Polymers TPP-140 Polypropylene, Homopolymer, 40% Talc Filled Polypropylene with 40% Talc Filler
Lucent Polymers TPP-230 Polypropylene, 30% Talc Filled, Impact Modified Polypropylene with 30% Talc Filler
Lucent Polymers TPP-240 Polypropylene, 40% Talc Filled, Impact Modified Polypropylene with 40% Talc Filler
Lucent Polymers TPP-310 Polypropylene, 10% Talc Filled, Impact Modified Polypropylene with 10% Talc Filler
Lucent Polymers TPP-320 Polypropylene, 20% Talc Filled, Impact Modified Polypropylene with 20% Talc Filler
Lucent Polymers TPP-340 Polypropylene, 40% Talc Filled, Impact Modified Polypropylene with 40% Talc Filler
Lucent Polymers PEI-100 Polyetherimide, General Purpose Polyetherimide (PEI)
Lucent Polymers POM-100 Acetal Copolymer, General Purpose, Injection Grade Acetal Copolymer, Unreinforced
Lucent Polymers POM-270 Acetal Copolymer, Easy Flow, Injection Grade Acetal Copolymer, Unreinforced
Lucent Polymers POM-900P Acetal Homopolymer, Easy Flow, Injection Grade Acetal Homopolymer, Unreinforced
Lucent Polymers PPC-210 Polypropylene, Impact Modified Polypropylene, Impact Modified; Molded/Extruded
Lucent Polymers PPC-220 Polypropylene, Impact Modified Polypropylene, Impact Modified; Molded/Extruded
Lucent Polymers PPC-320 Polypropylene, Impact Modified Polypropylene, Impact Modified; Molded/Extruded
Lucent Polymers PPH-110 Polypropylene, Homopolymer Polypropylene (PP)
Lucent Polymers TPO-1015 Thermoplastic Polyolefin Polyolefin