| Plastics Group Polifil® 625L Nylon 6/6 (DAM) |
Nylon 66, Unreinforced |
Polifil®
|
| Plastics Group Polifil® 627L Nylon 6/6 (DAM) |
Nylon 66, Unreinforced |
Polifil®
|
| Plastics Group Polifil® 628-13GF Glass Fiber-Reinforced Nylon 6/6 (DAM) |
Nylon 66, 20% Glass Fiber Filled |
Polifil®
|
| Plastics Group Polifil® 628-33GF Glass Fiber-Reinforced Nylon 6/6 (DAM) |
Nylon 66, 30% Glass Fiber Filled |
Polifil®
|
| Plastics Group Polifil® 628L Nylon 6/6 (DAM) |
Nylon 66, Unreinforced |
Polifil®
|
| Plastics Group Polifil® 71MR Mineral-Reinforced Nylon 6/6 (DAM) |
Nylon 66 |
Polifil®
|
| Plastics Group Polifil® 836L Nylon 6 (DAM) |
Nylon 6, Unreinforced |
Polifil®
|
| Plastics Group Polifil® 89MRGFHS Glass Fiber and Mineral Reinforced Nylon 6 (DAM) |
Nylon 6, Glass/Mineral Reinforced |
Polifil®
|
| Plastics Group Polifil® 930L Nylon 6 (DAM) |
Nylon 6, Unreinforced |
Polifil®
|
| Plastics Group Polifil® 930L-13GF Glass Fiber-Reinforced Nylon 6 (DAM) |
Nylon 6, 20% Glass Fiber Filled |
Polifil®
|
| Plastics Group Polifil® 930L-33GF Glass Fiber-Reinforced Nylon 6 (DAM) |
Nylon 6, 40% Glass Fiber Filled |
Polifil®
|
| Plastics Group Polifil® BS-70 70% Barium Sulfate Reinforced Polypropylene |
Polypropylene (PP) |
Polifil®
|
| Plastics Group Polifil® C-10 10% Calcium Carbonate-Reinforced Polypropylene |
Polypropylene with 10% Calcium Carbonate (CaCO3) Filler |
Polifil®
|
| Plastics Group Polifil® C-20 20% Calcium Carbonate-Reinforced Polypropylene |
Polypropylene with 20% Calcium Carbonate (CaCO3) Filler |
Polifil®
|
| Plastics Group Polifil® C-30 30% Calcium Carbonate-Reinforced Polypropylene |
Polypropylene with 30% Calcium Carbonate (CaCO3) Filler |
Polifil®
|
| Plastics Group Polifil® C-40 40% Calcium Carbonate-Reinforced Polypropylene |
Polypropylene with 40% Calcium Carbonate (CaCO3) Filler |
Polifil®
|
| Plastics Group Polifil® GFABS-10 10% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) |
Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled |
Polifil®
|
| Plastics Group Polifil® GFABS-20 20% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) |
Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled |
Polifil®
|
| Plastics Group Polifil® GFABS-30 30% Glass-Reinforced Acrylonitrile-Butadiene Styrene (ABS) |
Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled |
Polifil®
|
| Plastics Group Polifil® GFPC-20 20% Glass-Reinforced Polycarbonate |
Polycarbonate, 20% Glass Filled |
Polifil®
|
| Plastics Group Polifil® GFPP-40 40% Glass-Reinforced Polypropylene |
Polypropylene with 40% Glass Fiber Filler |
Polifil®
|
| Plastics Group Polifil® GFPPCC-30 30% Glass Reinforced Polypropylene |
Polypropylene with 30% Glass Fiber Filler |
Polifil®
|
| Plastics Group Polifil® GFPPCC-40 40% Glass Reinforced Polypropylene |
Polypropylene with 40% Glass Fiber Filler |
Polifil®
|
| Plastics Group Polifil® GFRMPPCC-30 30% Glass Reinforced Polypropylene, High Impact |
Polypropylene with 30% Glass Fiber Filler |
Polifil®
|
| Plastics Group Polifil® GFRMPPCC-40 40% Glass Reinforced Polypropylene, High Impact |
Polypropylene with 40% Glass Fiber Filler |
Polifil®
|
| Plastics Group Polifil® M-20 20% Mica-Reinforced Polypropylene |
Polypropylene with 20% Mica Filler |
Polifil®
|
| Plastics Group Polifil® M-40 40% Mica-Reinforced Polypropylene |
Polypropylene with 40% Mica Filler |
Polifil®
|
| Plastics Group Polifil® RMC-10 10% Calcium Carbonate-Reinforced Polypropylene, High Impact |
Polypropylene with 10% Calcium Carbonate (CaCO3) Filler |
Polifil®
|
| Plastics Group Polifil® RMC-20 20% Calcium Carbonate-Reinforced Polypropylene, High Impact |
Polypropylene with 20% Calcium Carbonate (CaCO3) Filler |
Polifil®
|
| Plastics Group Polifil® RMC-20V 20% Calcium Carbonate-Reinforced Polypropylene, High Impact, UV Stabilized |
Polypropylene with 20% Calcium Carbonate (CaCO3) Filler |
Polifil®
|
| Plastics Group Polifil® RMC-30 30% Calcium Carbonate-Reinforced Polypropylene, High Impact |
Polypropylene with 30% Calcium Carbonate (CaCO3) Filler |
Polifil®
|
| Plastics Group Polifil® RMC-40 40% Calcium Carbonate-Reinforced Polypropylene, High Impact |
Polypropylene with 40% Calcium Carbonate (CaCO3) Filler |
Polifil®
|
| Plastics Group Polifil® RMC-40V 40% Calcium Carbonate-Reinforced Polypropylene, High Impact, UV Stabilized |
Polypropylene with 40% Calcium Carbonate (CaCO3) Filler |
Polifil®
|
| Plastics Group Polifil® RMT-10 10% Talc-Reinforced Polypropylene, High Impact |
Polypropylene with 10% Talc Filler |
Polifil®
|
| Plastics Group Polifil® RMT-30 30% Talc-Reinforced Polypropylene, High Impact |
Polypropylene with 30% Talc Filler |
Polifil®
|
| Plastics Group Polifil® RMT-40 40% Talc-Reinforced Polypropylene, High Impact |
Polypropylene with 40% Talc Filler |
Polifil®
|
| Plastics Group Polifil® RP-ABS Acrylonitrile-Butadiene Styrene, Standard Version |
Acrylonitrile Butadiene Styrene (ABS), Molded |
Polifil®
|
| Plastics Group Polifil® RP-HDPE High Density Polyethylene |
High Density Polyethylene (HDPE), Injection Molded |
Polifil®
|
| Plastics Group Polifil® RP-LDPE Low Density Polyethylene |
Low Density Polyethylene (LDPE), Molded |
Polifil®
|
| Plastics Group Polifil® RP-PP Polypropylene, Black |
Polypropylene, Molded |
Polifil®
|
| Plastics Group Polifil® T-40 40% Talc-Reinforced Polypropylene |
Polypropylene with 40% Talc Filler |
Polifil®
|
| Plastics Group Polifil® 78MRGF Glass Fiber and Mineral Reinforced Nylon 6/6 (DAM) |
Nylon 66, Glass/Mineral Filled |
Polifil®
|
| Plastics Group Polifil® 82MR Mineral-Reinforced Nylon 6 (DAM) |
Nylon 6 |
Polifil®
|
| Plastics Group Polifil® GFPC-10 10% Glass-Reinforced Polycarbonate |
Polycarbonate, 10% Glass Filled |
Polifil®
|
| Plastics Group Polifil® GFPC-30 30% Glass-Reinforced Polycarbonate |
Polycarbonate, 30% Glass Filled |
Polifil®
|
| Plastics Group Polifil® GFPC-40 40% Glass-Reinforced Polycarbonate |
Polycarbonate, 40% Glass Filled |
Polifil®
|
| Plastics Group Polifil® GFPP-10 10% Glass-Reinforced Polypropylene |
Polypropylene with 10% Glass Fiber Filler |
Polifil®
|
| Plastics Group Polifil® GFPP-20 20% Glass-Reinforced Polypropylene |
Polypropylene with 20% Glass Fiber Filler |
Polifil®
|
| Plastics Group Polifil® GFPP-30 30% Glass-Reinforced Polypropylene |
Polypropylene with 30% Glass Fiber Filler |
Polifil®
|
| Plastics Group Polifil® GFPPCC-10 10% Glass Reinforced Polypropylene |
Polypropylene with 10% Glass Fiber Filler |
Polifil®
|
| Plastics Group Polifil® GFPPCC-20 20% Glass Reinforced Polypropylene |
Polypropylene with 20% Glass Fiber Filler |
Polifil®
|
| Plastics Group Polifil® GFRMPPCC-10 10% Glass Reinforced Polypropylene, High Impact |
Polypropylene with 10% Glass Fiber Filler |
Polifil®
|
| Plastics Group Polifil® GFRMPPCC-20 20% Glass Reinforced Polypropylene, High Impact |
Polypropylene with 20% Glass Fiber Filler |
Polifil®
|
| Plastics Group Polifil® RMT-20 20% Talc-Reinforced Polypropylene, High Impact |
Polypropylene with 20% Talc Filler |
Polifil®
|
| Plastics Group Polifil® RMT-40V 40% Talc-Reinforced Polypropylene, High Impact, UV Stabilized |
Polypropylene with 40% Talc Filler |
Polifil®
|
| Plastics Group Polifil® RP-ABS Acrylonitrile-Butadiene Styrene, High Flow Version |
Acrylonitrile Butadiene Styrene (ABS), Molded |
Polifil®
|
| Plastics Group Polifil® RP-HIPS High Impact Polystyrene |
Polystyrene, Impact Modified |
Polifil®
|
| Plastics Group Polifil® RP-PP Polypropylene, Molding Grade |
Polypropylene, Molded |
Polifil®
|
| Plastics Group Polifil® T-10 10% Talc-Reinforced Polypropylene |
Polypropylene with 10% Talc Filler |
Polifil®
|
| Plastics Group Polifil® T-20 20% Talc-Reinforced Polypropylene |
Polypropylene with 20% Talc Filler |
Polifil®
|
| Plastics Group Polifil® T-30 30% Talc-Reinforced Polypropylene |
Polypropylene with 30% Talc Filler |
Polifil®
|
| Plastics Group Polifil® RMT-20V 20% Talc-Reinforced Polypropylene, High Impact, UV Stabilized |
Polypropylene with 20% Talc Filler |
Polifil®
|