Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M 12034 Black 1/4" (6.4 mm) Polyurethane Foam

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF 3M 12034 Black 1/4" (6.4 mm) Polyurethane Foam.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance for tough duty gasketingChoice of thickness from low profile 1/16 inch to a gap-filling 1/2 inchLow VOC to help meet green goalsLow-outgassing for electronics applicationsChoice of five prelaminated adhesive formulations with good peel and shear strength for most surfaces including hard-to-bond plastics; all with performance at up to 250°FAvailable with or without adhesiveClean, easy die cutting and slittingLow minimum order quantitiesCustom slit widthsNon Adhesive foams are UL 94HBF, File E61941 Recognized CouponInformation provided by 3M
Physical Properties Metric English Comments
Density 0.240 g/cc
0.00867 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.345 MPa
50.0 psi
Elongation at Break 90 %
90 %
Compressive Strength 0.0241 - 0.0448 MPa
3.50 - 6.50 psi
Deflection
Tear Strength 0.700 kN/m
4.00 pli
Thermal Properties Metric English Comments
Minimum Service Temperature, Air 66.0 °C
151 °F
Long term
121 °C
250 °F
Short term
Users viewing this material also viewed the following: