3M Controltac™ 3545C Removable Graphic Film with Comply™ Adhesive

Category Polymer , Film
Manufacturer 3M
Trade Name Controltac™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Controltac™ 3545C Removable Graphic Film with Comply™ Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
4-mil white, opaque, polyolefin film; Chloride-free film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Air release channels for fast and easy application; Removable with heatInformation provided by 3M
Physical Properties Metric English Comments
Thickness 102 microns
4.00 mil
without adhesive
114 - 127 microns
4.50 - 5.00 mil
with adhesive
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.8 MPa
2000 psi
Peel Strength 0.193 - 0.228 kN/m
1.10 - 1.30 pli
Adhesion to Fruehauf pre-painted panels
0.351 - 0.403 kN/m
2.00 - 2.30 pli
Adhesion to Aluminum, anodized
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 38.0 °C
100 °F
Minimum Service Temperature, Air 4.00 °C
39.2 °F