Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ THV 815GZ Fluorothermoplastic Granules

Category Polymer , Thermoplastic , Fluoropolymer
Manufacturer 3M Dyneon™
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ THV 815GZ Fluorothermoplastic Granules.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Dyneon THV 815 GZ provides a balance of low permeation, thermal stability, and melt processability. IT can be used to prepare molded parts and extruded films, tubes, profiles, and wire coatings. It is useful for applications that require flexibility and good chemical resistance. This product processes at higher temperature than that of previous THV grades; therefore, the use of corrosion-resistant equipment is suggested.Information provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Melt Index of Compound 12 g/10 min

@Load 5.00 kg,
Temperature 265 °C
12 g/10 min

@Load 11.0 lb,
Temperature 509 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 29.0 MPa
4210 psi
ASTM D638
Elongation at Break 420 %
420 %
ASTM D638
Flexural Modulus 0.525 GPa
76.1 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
ASTM D4591
Descriptive Properties Value Comments
Form Pellets