Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchcal™ IJ5000 Reflective Graphic Film'

Category Polymer , Film
Manufacturer 3M
Trade Name ScotchCal™
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF 3M Scotchcal™ IJ5000 Reflective Graphic Film'.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
6-mil, enclosed lens, retroflective, flexible films; Pressure-sensitive adhesive; Permanent; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Version for screen printing, inkjet printing, and electrostatic imaging; Designed for excellent cutting and weeding with computer sign cutting equipment; For vertical, flat without rivets surfaces; Unprocessed film resists fuel vapor or occasional spillsInformation provided by 3M
Physical Properties Metric English Comments
Thickness 152 microns
6.00 mil
with adhesive
Mechanical Properties Metric English Comments
Peel Strength 0.456 kN/m
2.60 pli
Adhesion to Painted aluminum panels
0.649 kN/m
3.70 pli
Adhesion to FRP
0.841 kN/m
4.80 pli
Adhesion to Aluminum
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 29.0 °C
84.2 °F
Air and substrate, for flat surfaces without rivets
29.0 °C
84.2 °F
Air and substrate, for flat surfaces with rivets
38.0 °C
100 °F
Dry, flat surfaces without rivets
Minimum Service Temperature, Air 10.0 °C
50.0 °F
Dry, flat surfaces without rivets
10.0 °C
50.0 °F
Air and substrate, for flat surfaces without rivets
13.0 °C
55.4 °F
Air and substrate, for flat surfaces with rivets