A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D792
Melt Index of Compound 6.5 g/10 min
6.5 g/10 min
2.16/190; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.2 MPa
2200 psi
2"/min; ASTM D638
Elongation at Break 50 %
50 %
2"/min; ASTM D638
Flexural Modulus 0.586 GPa
85.0 ksi
at 1% secant modulus; ASTM D790
Impact Test 20.3 J

@Thickness 3.17 mm,
Temperature 23.0 °C
15.0 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ARM impact
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 48.0 °C
118 °F
ASTM D648
Flammability, UL94 V-2

@Thickness 1.50 mm
V-2

@Thickness 0.0591 in
V-2

@Thickness 6.00 mm
V-2

@Thickness 0.236 in
Descriptive Properties Value Comments
UV Stabilization UV-4