| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.28 g/cc | 0.0462 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0010 cm/cm | 0.0010 in/in | MD; ASTM D955 |
| Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 118 | 118 | ASTM D785 |
| Tensile Strength at Break | 95.01 MPa | 13780 psi | ASTM D638 |
| Tensile Strength, Yield | 95.01 MPa | 13780 psi | ASTM D638 |
| Elongation at Break | 3.0 % | 3.0 % | ASTM D638 |
| Elongation at Yield | 2.0 % | 2.0 % | ASTM D638 |
| Tensile Modulus | 6.399 GPa | 928.1 ksi | ASTM D638 |
| Flexural Strength | 132.0 MPa | 19140 psi | ASTM D790 |
| Flexural Modulus | 9.9981 GPa | 1450.1 ksi | ASTM D790 |
| Izod Impact, Notched | 0.448 J/cm | 0.840 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 97.2 °C | 207 °F |