Akro-Plastic Akromid® B3 GF 30 S1 NAT. (1383) PA, Cold-Impact Resistant, 30% Glass Filled, Natural

Category Polymer , Thermoplastic , Nylon
Manufacturer Akro-Plastic
Trade Name Akromid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akro-Plastic Akromid® B3 GF 30 S1 NAT. (1383) PA, Cold-Impact Resistant, 30% Glass Filled, Natural.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
The outstanding characteristic is the reduction of the normally common cooling brittleness at low temperatures. Here, AKROMID A has set a course with special combinations like high heat stabilization for the engine compartment or very good UV- resistance for the out door area. However, calcium chloride is critical with regard to PA6.6. In combination with anti-freeze containing window cleaning fluid, an ugly white film is emerging on the surface. Main applications are window cleaning fluid valves, head light cleaning units, wiper end caps, bezels etc. in the front area of the automobile.Information from Akro-Plastic
Mechanical Properties Metric English Comments
Tensile Stress 125 MPa
18100 psi
Charpy Impact, Notched 3.50 J/cm²
16.7 ft-lb/in²