| Category | Ceramic , Oxide |
| Manufacturer | Alliance LLC |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Alliance C-8 Strontium Ferrite Ceramic Magnetic Material.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 4.80 - 5.00 g/cc | 0.173 - 0.181 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Vickers | 450 - 580 | 450 - 580 | |
| Tensile Strength, Ultimate | 20.0 - 50.0 MPa | 2900 - 7250 psi | |
| Modulus of Elasticity | 150 GPa | 21800 ksi | |
| Flexural Strength | 55.0 MPa | 7980 psi | |
| Compressive Strength | 700 MPa | 102000 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
| CTE, linear, Transverse to Flow | 8.00 µm/m-°C @Temperature 23.0 °C |
4.44 µin/in-°F @Temperature 73.4 °F |
|
| Maximum Service Temperature, Air | 350 °C | 662 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | >= 1.00 ohm-cm | >= 1.00 ohm-cm | |
| Magnetic Coercive Force, Hc | 2950 Oe | 2950 Oe | |
| 3100 Oe | 3100 Oe | Intrinsic | |
| Magnetic Remanence, Br | 3900 Gauss | 3900 Gauss | |
| Magnetic Maximum Energy Product, BH | 3.6 MGOe | 3.6 MGOe | |
| Curie Temperature | 450 °C | 842 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Reversible Temp Coef., Bd | -0.20 %/°C | |
| Reversible Temp Coef., Hd | +0.35 %/°C | |
| Temperature Coefficient, Br | -0.18 %/°C | (20-100°C) |
| Temperature Coefficient, Hci | +0.4 %/°C | (20-100°C) |