AorTech Biomaterials ECSil™ 70A Biomedical Carbonate Silicone Pellets

Category Polymer , Thermoplastic , Polyurethane, TP , Silicone Polyurethane, Ether Based
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AorTech Biomaterials ECSil™ 70A Biomedical Carbonate Silicone Pellets.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Elast-Eon™ Carbonate Silicone (ECSil™) is a family of next generation biomedical polymers. ECSil™ is finding strong interest in cardiac pacing leads, orthopaedics, spinal discs, and generally any application where the device requires a very high level of mechanical performance. ECSil™ is soluble in both THF and DMAc; it is supplied in pellet form.
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength at Break 25.0 MPa
3630 psi
Elongation at Break 750 %
750 %
Modulus of Elasticity 0.00800 GPa
1.16 ksi
Tear Strength 60.0 kN/m
342 pli