Aremco AREMCOLOX™ 502-1900-YTZP Dense Yttria Stabilized Zirconium Oxide

Category Ceramic , Oxide , Zirconium Oxide
Manufacturer Aremco
Trade Name AREMCOLOX™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco AREMCOLOX™ 502-1900-YTZP Dense Yttria Stabilized Zirconium Oxide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
This grade offers a high flexural strength for a zirconia. The fine grain size lends itself to be used in cutting tools where a very sharp edge can be achieved and maintained due to its high wear resistance. Also provides excellent mechanical strength, corrosion and thermal shock resistance, impact toughness, and very low thermal conductivity. Used for structural components, wear parts, fiber optic ferrules and sleeves, oxygen sensors, and solid oxide fuel cells (SOFC).
Physical Properties Metric English Comments
Specific Gravity 5.85 g/cc
5.85 g/cc
Porosity 0.00 %
0.00 %
Mechanical Properties Metric English Comments
Hardness, Mohs 8.0
8.0
Flexural Strength 207 MPa
30000 psi
Compressive Strength 2500 MPa
363000 psi
Thermal Properties Metric English Comments
CTE, linear 10.4 µm/m-°C
5.80 µin/in-°F
Thermal Conductivity 2.20 W/m-K
15.3 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 1800 °C
3270 °F
Electrical Properties Metric English Comments
Dielectric Constant 29

@Frequency 1.00e+6 Hz
29

@Frequency 1.00e+6 Hz
Dielectric Strength 8.98 kV/mm
228 kV/in
Dielectric Loss Index 0.0010

@Frequency 1.00e+6 Hz
0.0010

@Frequency 1.00e+6 Hz